Size chart
Copper tube outer diameters in inch and mm; insulated OD given separately for 9 mm and 13 mm PE.
| Size | Liquid line OD | Gas line OD | OD with 9 mm insulation | OD with 13 mm insulation | Min. bend radius |
|---|---|---|---|---|---|
| 1/4" × 3/8" | 6.35 mm | 9.52 mm | 24.4 / 27.5 mm | 32.4 / 35.5 mm | 38 mm |
| 1/4" × 1/2" | 6.35 mm | 12.70 mm | 24.4 / 30.7 mm | 32.4 / 38.7 mm | 51 mm |
| 1/4" × 5/8" | 6.35 mm | 15.87 mm | 24.4 / 33.9 mm | 32.4 / 41.9 mm | 63 mm |
| 3/8" × 5/8" | 9.52 mm | 15.87 mm | 27.5 / 33.9 mm | 35.5 / 41.9 mm | 63 mm |
| 3/8" × 3/4" | 9.52 mm | 19.05 mm | 27.5 / 37.1 mm | 35.5 / 45.1 mm | 76 mm |
| 1/2" × 3/4" | 12.70 mm | 19.05 mm | 30.7 / 37.1 mm | 38.7 / 45.1 mm | 76 mm |
Why insulation matters
Prevents condensation
If the cold gas line touches ambient air, water droplets form on it; closed-cell PE prevents this and protects walls and ceilings.
Preserves efficiency
Heat gain along the run drops and the compressor works less; especially on long, sun-exposed runs this saves energy.
Withstands the outdoors
The UV-resistant white skin does not yellow or crack in the sun; extra protection with trunking or tape is still recommended outdoors.
Flame retardant
The insulation and PE skin are flame-retardant; they do not sustain a flame and add to fire safety in indoor installations.
Easy installation
Two pipes in one jacket: no separate insulation wrapping on site, shorter installation time.
Installation and brazing advice
Bending
- Bend radius should be at least 4× the tube OD; tight bends narrow the cross-section.
- Use a bending spring or mechanical bender on 1/2" and larger tube.
- Do not pull the coil straight off the ground; roll the ring open, otherwise the tube twists.
Cutting and flaring
- Use a tube cutter; a saw leaves swarf. Deburr the bore after cutting.
- For R410A / R32 use a 45° flare and the torque values given by the unit manufacturer.
Brazing
- Purge a low flow of nitrogen through the tube while brazing; it prevents oxide scale.
- Slide the insulation back at least 10 cm from the joint; push it back after cooling.
- Use phosphor–silver alloy rod for copper-to-copper joints; no flux needed.
Commissioning
- Pressure test with nitrogen, then pull a vacuum of at least −0.1 MPa (below 750 microns).
- Remove the end caps just before installation; do not leave open tube in a humid environment.
Frequently asked questions
Can you produce custom sizes or coil lengths?
Yes. We produce twin and single pipe from 1/4" to 3/4" with 9 or 13 mm insulation in coil lengths to your request. Send the size and quantity and we share a quote and lead time.
Do you produce under our own brand?
Yes. Your brand name and logo are printed on the white PE jacket; label and carton design are prepared to your request.
How is shipping handled?
Coils are shipped in cartons or on pallets with capped ends. Road, sea or air freight; export documents and certificate of origin are prepared by us.
Is the pipe suitable for R32?
Yes. Our tube is produced for high-pressure refrigerants such as R32 and R410A; follow the unit manufacturer’s torque values when flaring.